Pyrotek Pyrotherm TF-19 Lightweight, non-RCF insulation board for ovens, furnaces, kilns and vessels
Material Notes: Pyrotherm TF-19 is a high-temperature board providing high strength and excellent workability. It is composed of mineral fiber and selected mineral additives. Applications - Pot cradle insulation (for Alcoa A-697 pots)
- Precipitators
- Dryers
- Ducts and breeching
- Utility boilers
- Furnaces
- Kilns
Advantages - Excellent mechanical strength in non-fired condition
- Refractory ceramic fiber free
- Low thermal conductivity
- Use of large-size boards to reduce labor costs
- Material can be cut quickly by hand with knife or saw for fabrication and application on the job
Information provided by Pyrotek.
| Available Properties |
- Density
- Modulus of Rupture
- Compressive Strength
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|