Reade Advanced Materials Chromium Trioxide (CrO3)
Subcategory: Oxide, Other; Oxide
Key Words: CrO3, chromic acid, chromium oxide
Material Notes: Description: A hexavalent chromium compound and a powerful oxidizing agent. Health effects are limiting applications. Uses: Chromium plating, wood preservation industry, anodizing aluminum, corrosion resistance applications, sealing phosphate coatings applied to iron or steel, bright dipping of brass, acid cleaning of Al and Mg and organic synthesis. Physical Properties Available: Various granulations available from 3-6 mm fused pieces down to as small as nanoparticles. Information provided by Reade Advanced Materials.
| Available Properties |
- Specific Gravity
- pH
- Molecular Weight
- Melting Point
|
|
|
|