Reade Advanced Materials Diopside Powder (CaMg(CO3)2 and CaMg(SiO3)2)
Key Words: CaMg(CO3)2 and CaMg(SiO3)2, Calcium-magnesium silicate, calcium-magnesium pyroxene, malacolite, alalite
Material Notes: Description: A naturally mined mineral that is relatively difficult to source. Low-iron grades have use in glass manufacture, whiteware bodies, glazes, and welding rod coatings. Physical Properties Available: Lump or powder (100 mesh x down, 250 mesh by down or 400 mesh by down) Information provided by Reade Advanced Materials.
|
|
|