Reade Advanced Materials Garnet Powder (Fe3Al2(SiO4)3)
Subcategory: Oxide, Silicon; Oxide
Key Words: Fe3Al2(SiO4)3, Iron aluminum silicate
Material Notes: Description: A group of iron aluminum silicate homogeneous minerals having similar properties. Non-hygroscopic, sharp angular shape, inert, slightly magnetic, not soluble in water, translucent, friable to tough, and contains no free chemicals. All oxides and dioxides are combined chemically as follows: Fe2O3Al2(SiO4)3. The iron and aluminum are partially replaceable by calcium, magnesium and manganese. There are three types- aluminum garnet, iron garnet & chromium garnet. Uses:
Abrasive applications, water jet cutting, water filtration, tumbling media, non-skid surfaces, and semi-precious stone. Physical Properties Available: Sintered pieces, targets, granules and various powder sizings Information provided by Reade Advanced Materials.
| Available Properties |
- Specific Gravity
- Bulk Density
- Hardness, Mohs
- Melting Point
- Refractive Index
- Color
- Crystal Structure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|