Reade Advanced Materials Indium-Tin Oxide (ITO) Powder (In203:Sn02)
Subcategory: Oxide, Other; Oxide
Key Words: In203:Sn02, ITO, Indium tin oxide, Vacuum Deposition Grade, 99.999%
Material Notes: Description: Indium oxide doped with tin oxide, ITO, is used to make transparent conductive coatings. Thin film layers can be deposited by electron-beam evaporation or sputtering. Roll or web coating on polymer substrates is done by magnetron or other techniques of sputtering. End uses of ITO are: Flat panel display applications; ITO glass manufacturing techniques; electroluminescent display applications; plasma display panel applications; electrochromic display applications; field emission display applications; new flat panel display technologies; and heat reflecting mirrors. Information provided by Reade Advanced Materials.
| Available Properties |
- Density
- Molecular Weight
- Melting Point
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|