Reade Advanced Materials Tungsten Oxide Powder (WO2 and WO3)
Subcategory: Oxide, Other; Oxide
Key Words: WO2, WO3
Material Notes: Description: Tungsten oxide is obtained from the minerals scheelite, wolframite, ferberite. It is insoluble in H2O and acids, but soluble in hot alkalis. Used in the manufacture of tungsten and tungstates, in alloys, in fire-proofing fabrics and as a ceramic pigment. Physical Properties Available: Targets, pieces, and powder Information provided by Reade Advanced Materials.