Reade Advanced Materials Zirconium Silicate (Zircon) Powder (ZrSiO4)
Subcategory: Oxide, Silicon; Oxide, Zirconium; Oxide
Key Words: ZrSiO4
Material Notes: Description: A fine white mineral powder that is chemically inert and stable to very high temperatures. Insoluble in water, dilute acids and hot concentrate sulfuric acid. Used as a primary source for investment casting shell molds, foundry cores, metal chills, ladle brick, welding rod coatings, abrasive cleaning, and mold washes. Physical Properties Available: -50+270 mesh, -60+200 mesh, -200 mesh and -325 mesh Information provided by Reade Advanced Materials.
Available Properties |
- Specific Gravity
- Bulk Density
- Molecular Weight
- Hardness, Mohs
- Melting Point
- Color
|
|
|
|