Schott AF 45 Thin Borosilicate Glass

 

Subcategory: Glass; Oxide, Silicon; Optical; Oxide

Material Notes:
AF 45 is an alkali-free modified borosilicate glass with a high content of BaO and Al2O3. AF 45 with, its specific properties and large range of different thicknesses with tight tolerances, is exceptionally well suited for a number of applications including: liquid crystal displays, electroluminescent displays, CCD covers, hybrid circuits and solar cells. Due to a special down draw production process, AF 45 glass sheets are marked by fire-polished surfaces; this glass type can be used without ground and polished surfaces. AF 45 offers excellent thermal resistance for high temperature applications up to approximately 600°C.

Information provided by SCHOTT North America.

Available Properties
  • Density
  • Thickness
  • Hardness, Knoop
  • Modulus of Elasticity
  • Poissons Ratio
  • Shear Modulus
  • Volume Resistivity
  • Dielectric Constant
  • Dissipation Factor
  • CTE, linear 20°C
  • Thermal Conductivity
  • Thermal Conductivity at Elevated Temperature
  • Transformation Temperature, Tg
  • Softening Point
  • Annealing Point
  • Refractive Index
  • Transmission, Visible
  • Abbe Value
  • Dispersion
  • Strain Point
  • Stress Optical Coefficient
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。