Schott Band Pass Filter BG12
Subcategory: Glass; Optical; Filter
Close Analogs: BG4, BG7, BG3, BG18, BG23, BG24A, BG25, BG26, BG28, BG38, BG39, BG40, BG42, RG9, UG1, UG5, UG11, VG6, VG9, VG14
Key Words: DIN BP 409/140
Material Notes: Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
| Available Properties |
- Density
- Acid Class, SR
- Alkali Class, AR
- Stain Resistance Class, FR
- CTE, linear 20°C
- CTE, linear 250°C
- Transformation Temperature, Tg
- Refractive Index
- Transmission, Visible
- IR Transmittance
- UV Transmittance
- Reflection Coefficient, Visible (0-1)
|
|
|
|