Sinotek Materials Spherical Graphite ZSG-25
Subcategory: Graphite; Carbon
Material Notes: Also called"Potato Graphite", Spherical Graphite is ideal cathode material for lithium ion batteries. Using high quality natural flake graphite as raw material, our company adopts a series of unique shaping, classification, and purification technologies to produce high quality Spherical Graphite. Our products are well crystallized, have high-roundness and are of stable quality; its first discharge capability is up to 360mAh/g, and the recharge and discharge efficiency is up to 80 percent.Information provided by Sinotek
| Available Properties |
- Density
- Particle Size
- Specific Surface Area
- Moisture Content
- Discharge Volume, mAh/g
|
|
|
|