Sinotek Materials Graphite Emulsion MD-2
Subcategory: Graphite; Carbon; Ceramic
Material Notes: The graphite emulsion is forged with patented equipment and a unique recipe. It is an ideal lubricant for high-temperature demoulding in hot processing of non-ferrous metal. The superior products are used in aviation and space flight as well as extrusion of warheads and cartridge cases. With ideal high-temperature lubricity and cohesiveness, it makes demoulding easy. It is chemically stable, non-corrosive and non-toxic. It can improve the moulding quality and remarkably prolong the life of moulds. Examples of application include drop forging, roll forging, gear rough and finish forge.Information provided by Sinotek
| Available Properties |
- Solids Content
- Graphite Content %
- Subsidency After 3 hrs, 20 Times of Dilution %
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|