Sinotek Materials Packing Expanded Graphite Yarns
Subcategory: Graphite; Carbon
Material Notes: Expanded graphite yarns are made of twists of low-sulphur expanded combined with reinforcing materials, and are suitable for weaving of expanded graphite braided packings. There is a wide variety of reinforcing materials used in the yarn twisting of different working conditions, with include cotton yarn, fiberglass, carbonized fiber, wires of nickel alloy or stainless steel or copper.Information provided by Sinotek