Sinotek Materials Packing Carbon Fiber with Graphite
Subcategory: Carbon Fiber; Graphite; Carbon
Material Notes: The packing is woven of strong carbon fiber after softening treatment and impregnation with the mixture of fine graphite powder, PTFE dispersion and lubricant. Being strong, static and heat-conductive, it is widely used with revolving or reciprocating pumps, where media of chemical corrosion and grains of particles exist.Information provided by Sinotek
| Available Properties |
- pH
- Maximum Service Temperature, Air
- Max Working Pressure, MPa
|
|
|
|