Sinotek Materials Tungsten Disulfide Powder High-Pure
Subcategory: Sulfide/Chalcogenide; Ceramic/Metallic Coating; Ceramic
Material Notes: Tungsten Disulfide (WS2) powder mainly has application in spraying, coating, carbon material, all sorts of grease, lubricating oil, friction materials and catalyzers. Tungsten Disulfide has good resistance to corrosion, however cannot avoid corroding base materials completely. This product is chemically inert, non-magnetic, and is available in blue and grey. This product is processed to meet military specification DOD-L-85645.Information provided by Sinotek
| Available Properties |
- Density
- Thickness
- Hardness, Rockwell C
- Coefficient of Friction
- Coefficient of Friction, Static
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Load Capacity psi
- Purity WS2 wt%
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|