Skamol ISOPERLOR 550P Perlite Insulating Brick & Block
Subcategory: Oxide, Silicon; Oxide, Titanium; Oxide, Aluminum; Oxide
Material Notes: ISOPERLOR perlite insulating bricks & blocks have the following characteristics: - Max. service temperature 900°C (1652°F)
- Back-up insulation only
- Excellent insulating properties
- Very lightweight and highly porous
- Widely used for lining aluminum reductions cells due to their high resistance to cryolite bath, molten aluminum and fluoride gas exposure
Information provided by Skamol.
| Available Properties |
- Bulk Density
- Loss On Ignition
- Porosity
- Permeability
- Modulus of Rupture
- Compressive Strength
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Shrinkage
- Change After Fluoride Gas Exposure
- Color
- Creep in Compression
- Pyrometric Cone Equivalent
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|