Skamol V-1100 (475) Vermiculite Insulating Slab

 

Subcategory: Oxide, Silicon; Oxide, Titanium; Oxide, Aluminum; Oxide

Material Notes:
SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics:

  • Max. service temperature: Up to 1150°C (2102°F)
  • Hot-face applications or back-up insulation of all refractory constructions
  • Excellent insulating value
  • High mechanical strength
  • Good thermal shock resistance
  • Can be used in furnaces with reducing atmospheres due to their high resistance to carbon monoxide and hydrocarbons
  • Several grades available in various combinations of bulk density, insulation properties and compressive strength
  • A variety of uses in high-temperature kilns and furnaces, combustion plants, boilers as well as in hearth and heating appliances
  • High-density grade VIP-12 has a good resistance to cryolite and fluorides, which makes it particularly suitable for uses within the primary aluminum industry.

Information provided by Skamol.

Available Properties
  • Bulk Density
  • Loss On Ignition
  • Porosity
  • Modulus of Rupture
  • Compressive Strength
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Thermal Conductivity at Elevated Temperature
  • Maximum Service Temperature, Air
  • Shrinkage
  • Color
  • Pyrometric Cone Equivalent
  • Resistance to Thermal Shock
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。