Skamol M-20 Insulating Mortar
Subcategory: Oxide, Silicon; Oxide, Titanium; Oxide, Aluminum; Oxide
Material Notes: SKAMOL insulating mortars have the following characteristics: - Max. service temperature: Up to 1150°C (2102°F)
- Dry-mix mortars designed for use with Skamol insulating bricks/blocks and slab grades in various applications
- Good insulation values
- Outstanding bonding properties within max. service temperature range
- Water-retentive properties for quick and easy laying of dry bricks/blocks/slabs.
- Combined air and heat-setting.
Information provided by Skamol.
| Available Properties |
- Bulk Density
- Loss On Ignition
- Maximum Service Temperature, Air
- Moisture Content
- Binder
- Mixing Water Usage
- Package Weight
- Pyrometric Cone Equivalent
- Recommended Joint Thickness
- Setting Mechanism
- Type
- Usage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|