Skamol SKAMOCAST 112-80 Insulating Castable
Subcategory: Oxide, Silicon; Oxide, Titanium; Oxide, Aluminum; Oxide
Material Notes: SKAMOL insulating castables have the following characteristics: - Max. service temperature: Up to 1100°C (2102°F)
- Back-up insulation or hot-face uses
- For casting and gunning
- Products are based on fired Moler aggregates, refractory materials, or exfoliated vermiculite
- Effective insulation
- Quick and economical installation
- Used as monolithic heat insulation in a wide range of industrial kilns and furnaces, boilers, chimneys, and flues
- The Vermicast grades are favored as infill in aluminum reduction cell cathodes due to their non-wetting capacity to molten metal and good bath resistance.
Information provided by Skamol.
| Available Properties |
- Bulk Density
- Loss On Ignition
- Porosity
- Compressive Strength
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Shrinkage
- Pyrometric Cone Equivalent
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|