Skamol SICAL Mortar Silicon Carbide Mortar
Subcategory: Carbide; Oxide, Silicon; Oxide, Aluminum; Oxide
Material Notes: Sical mortar has the following characteristics: - Max. service temperature 1350°C (2462°F)
- Good adherence to SiC bricks
- High SiC content
- High content of fines
- Easy to handle
Information provided by Skamol.