SPHERE ONE EXTENDOSPHERES™ 350 Hollow Spheres
Subcategory: Additive/Filler for Polymer; Oxide
Material Notes: EXTENDOSPHERES™ hollow spheres are efficient, lightweight additives for most resin systems. When extendospheres™ replace heavier, more expensive components on an equivalent volume basis, they can reduce raw material costs as well as density.Applications: EXTENDOSPHERES™ 350 hollow spheres are a standard grade. They are recommended for use in cement, grout, sealants, roofing compounds, PVC and latex flooring. They can also be used in high mil-build industrial coatings and mastics. Information provided by Sphere One Inc.
| Available Properties |
- Density
- Bulk Density
- Particle Size
- Hardness, Mohs
- Compressive Strength
- Maximum Service Temperature, Air
- Color
- Physical Form
- Shell Thickness
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|