SPHERE ONE EXTENDOSPHERES™ SL-150 Hollow Spheres
Subcategory: Additive/Filler for Polymer; Oxide
Material Notes: EXTENDOSPHERES™ SL are white, low-cost, low-density ceramic hollow spheres.Applications: With a density of 0.73 g/cc and a crush strength of 3,000 psi, these hollow spheres are ideal for use in coatings, sealants, caulks and other applications where low shrinkage, lightweight and white particles are desired. Information provided by Sphere One Inc.
| Available Properties |
- Density
- Bulk Density
- Particle Size
- Hardness, Mohs
- Compressive Strength
- Maximum Service Temperature, Air
- Color
- Physical Form
- Shell Thickness
|
|
|
|