Sellar Ceramite® SFR Wear Resistant Castable

 

Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide

Material Notes:
Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world wide, both as mortars and as various precast components. Ceramite can easily be mixed, cast and shaped in any size and is thus comfortably to work with in-situ. Ceramite can be used in within a wide range of temperatures and applications exposed to thermal shock conditions in industries like for example aluminum, cement and ferro.

Applications: Floor Tile, Hearth/Furnace Tile, Furnace Sills & Doors, Lintels, Pipe and Duct Linings, Feed Tubes, Troughs/Launders, Ladles, Dampers, Nozzle Blasters, Crucible Linings, Vortex, Burner Tip Cooler Plates, Nose Ring, Electrical Insulation, Cold Wear Areas

Specific Notes on This Grade: A castable combining good mechanical and thermal properties. Extremely low thermal expansion. Mainly used in aluminum and zinc industries. References al launders, crucibles and other areas in contact with molten metal.

Information provided by Stellar Canada.

Available Properties
  • Bulk Density
  • Porosity
  • Modulus of Rupture
  • Flexural Strength
  • Compressive Strength
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Application
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。