Saint-Gobain Chemfab® 313X PTFE Coated Fiberglass Conveyor Belting
Subcategory: Glass Fiber
Material Notes: Description: General Notes on Saint Gobain Belting Products: Saint Gobain Performance Plastics developed its belting materials for applications that require superior release characteristics, permeability for rapid drying, dimensional and thermal stability, and the dynamic strength to stand up to the most rigorous operating conditions. The unique behavior of the materials results in a product that is more practical and cost-effective than conventional belting materials. Release Properties: The release characteristics of PTFE are superior to those of any other high-temperature material. This non-stick property is retained over a full range of operating temperatures. Permeability: Our belting combines a maximum amount of open area with good mechanical strength. The result is a very high level of controlled air flow through the belt, maximizing the rate of drying. Dimensional Stability: The woven reinforcement results in an elongation of approximately 1% under normal mechanical loading, even at temperatures of 550°F. Length distortion is exceptionally low, while width rigidity and stability are enhanced by the high modulus of the reinforcement. Thermal Stability: Chemfab® brand belting may be used continuously at temperatures up to 550°F without reducing its performance. Dynamic Stability: Our belting has been subjected to static and dynamic tests which indicate that it can withstand all normal operating conditions affecting service life. Chemical Resistance: PTFE surfaces are unaffected by most chemicals and solvents.
Notes on 313X PTFE Coated Fiberglass Conveyor Belting: Chemfab® 313X is a belting product used in applications that reqwuire high strength and low elongatiuon. This material has inherent stability that enhances its ability to resist ridging, puckering and creasing. The surface is textured because of the use of large yarns in the fiberglass substrate. The substrate is fiberglass and the coating material is PTFE (PTFE = polytetrafluoroethylene). Material is non-porous. All data based on a 0.024 inch test sample. Information provided by Saint Gobain Performance Products.
| Available Properties |
- Density
- Elongation at Yield
- Tear Strength Test
- Tear Strength
- Weight (oz/yd^2)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|