Saint-Gobain Chemfab® TCK® 800 High-Strength Leno Weave Small Open Mesh Belting Material
Subcategory: Glass Fiber
Material Notes: Description: General Notes on Saint Gobain Chemfab® TCK® Open Mesh Belting Products: TCK belting products are PTFE (PTFE = polytetrafluoroethylene) coated Kevlar®, a high-temperature aramid fiber that offers an extremely high strength-to-weight ratio. TCK is an excellent fabric for use in high moisture environments, for applications subjected to severe flexing, or for when added durability is required. Dimensional Stability: The Kevlar® base of TCK keeps stretch or shrinkage to less than 1% under normal operating tensions (3 to 10 pounds per inch of width) and temperatures up to 500°F. TCK belting has excellent resistance to flex fatigue. Release Properties: The release properties of TCK exceed those of any other available belting material. TCK is unique because of its low coefficient of friction. Chemically Resistant: The PTFE coating envapsulates the Kevlar® belting carcass and enhances its useful service life. Light Weight: The inherent strength of the Kevlar® filament provides durable belting at a fraction of the weight of other materials. Less power is required to move TCK belting (and the products moved). High Strength: Kevlar®, the filament base of the belting carcass, is stronger than steel on a pound-for-pound basis. Flex Fatigue Resistant: The unequaled strength of TCK, combined with its excellent flex fatigue properties, means TCK belting can be used on small pulley diameters for a long in-use life span. High Thermal Capability: At temperatures of up to 500°F, TCK belting continues to maintain its high performance profile. Low Thermal Mass: TCK belting (including the seam areas) quickly dissipates heat with low heat sink properties. Fabrication Technology: Saint-Gobain Performance Plastics belt seams have been specifically engineered to reduce the flex fatigue failure. Substantially reduced flex fatigue means longer belt life. Notes on TCK® 800 Leno Weave Small Open Mesh Belting Material: TCK 800 is a high-strength belting product. It is a Leno weave, open mesh material intended for use in forced hot air dryers. It has a small mesh opening, which is well suited for conveying small products. All data based on a 0.034 inch test sample. Information provided by Saint Gobain Performance Products.
| Available Properties |
- Density
- Elongation at Yield
- Tear Strength
- Weight (oz/yd^2)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|