Saint-Gobain Chemfab® Anti-Static PTFE-Coated Glass 5
Subcategory: Glass Fiber
Material Notes: Description: Chemfab® Anti-static Series is a high quality PTFE-coated glass fabric that can be used for release sheets, belting, or other applications requiring the dissipation of static electricity. All data based on a 0.005 inch test sample. Information provided by Saint Gobain Performance Products.
| Available Properties |
- Density
- Tear Strength Test
- Tear Strength
- Surface Resistivity per Square
- Weight (oz/yd^2)
|
|
|
|