Sylvania SA201 Tungsten & Chrome Based Thermal Spray Powder
Subcategory: Carbide; Tungsten Alloy; Ceramic/Metallic Coating
Material Notes: General DescriptionWC and Co powders are agglomerates to the specifications herein. The WC particles in the cobalt matrix are less than 20 micrometers and average 2-5 micrometers. The resulting agglomerates are very homogeneous. The WC-12Co powder provides a dense wear-resistant sprayed coating with very good surface smoothness. This powder can be combined with other powders such as nickel alloys to improve the density and the surface finish. Applications - Thread Guides
- Screw Conveyors
- Jet-Engine Components
- Pump Parts
| Available Properties |
- Bulk Density
- Particle Size
- Particle Mesh Size
- Hall Flow, seconds/50g
|
|
|
|