Sylvania SD252 Tungsten & Chrome Based Thermal Spray Powder
Subcategory: Carbide; Tungsten Alloy; Ceramic/Metallic Coating
Material Notes: General DescriptionSD252 is plasma densified tungsten carbide-cobalt spray powder, designed for use as a wear resistant coating. The major constituent is W2C. There is also some WC, as well as complex Co-W-C compounds. Its flow characteristics are excellent and the apparent density is high. Applications - Thread Guides
- Screw Conveyors
- Jet-engine Components
- Pump Parts
| Available Properties |
- Bulk Density
- Particle Size
- Hall Flow, seconds/50g
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|