Thermal Ceramics Cerachrome Blanket
Material Notes: Made from spun alumina-silica-chromia fiber, Cerachrome Blanket is well suited for hot face lining applications where higher temperatures are encountered, such as soaking pit covers, reheat and forging furnaces. Cerachrome Blanket with its chromia-stabilized chemistry offers improved long term shrinkage characteristics over zirconia containing blankets such as Cerachem. Cerachrome Blanket effectively fills the gap between zirconia blankets and high alumina products.Military Specifications and Approvals: Mil-I-23128A- 3, 6 pcf blanketMil-I-24244- all blanketsMil-I-23128B- 6, 8 pcf blanketInformation provided by Thermal Ceramics
| Available Properties |
- Density
- Thickness
- Thermal Conductivity at Elevated Temperature
- Melting Point
- Maximum Service Temperature, Air
- Other Element Content
- Water Leachable Elements on Surface of Fiber, PPM
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|