Thermal Ceramics Kaomat SL Blanket
Subcategory: Kaolin
Material Notes: Thermal Ceramics Kaomat insulation is a non-woven needle-felted "E" fiberglass mat. Kaomat is an economical insulating material used extensively in both the marine and commercial insulation markets. It is noncombustible, chemically stable, resists corrosion and is certifiable to MIL-I-24244 and NRC 1.36.Features:No “shot” blanket, Excellent dimensional stability, High tensile strength, Available in module form. Applications:Asbestos replacement, Steam and gas turbine blanket, Insulation of marine exhaust systems, Low temperature (<1200°F {649°C}) insulation, Aluminum homogenizing furnaces, “No-shot” furnace linings. Information provided by Thermal Ceramics
| Available Properties |
- Density
- Thickness
- Tensile Strength, Ultimate
- Thermal Conductivity at Elevated Temperature
- Melting Point
- Maximum Service Temperature, Air
- Shrinkage
- Fiber Diameter, microns
- Fiber Length, cm
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|