Thermal Ceramics Kaowool S Blanket Strip
Subcategory: Kaolin
Material Notes: Thermal Ceramics Kaowool® Strip products are cut from either Kaowool Blanket, Blanket S, Cerablanket®, or Cerachem® Blanket. These products are available in many forms and lengths depending upon the application. They have low thermal conductivity, low heat storage capacity, and are extremely resistant to thermal shock.Blanket strip products are highly efficient insulators. These products have low shot content which allows more usable fiber for your insulating dollar. Blanket strip products have longer fibers which give them high tensile strength and resiliency to withstand vibration and physical abuse. Blanket strip products are self-supporting and will not separate, sag, or settle. Blanket strips are available in a wide variety of widths, thicknesses, densities, and chemistries. This allows the user to select the proper product form for an application with a minimum of scrap and labor to install the strip. Blanket strip products have a wide variety of uses including packing for modules, expansion joints, and gaskets. Features: Available in a wide variety of widths, thicknesses, and densities Available in all Blanket compositionsApplications: Expansion jointsHigh-temperature filtrationGaskets Acoustical service for missiles, rockets, and jet enginesHigh-temperature insulationPacking stripsInformation provided by Thermal Ceramics
| Available Properties |
- Density
- Thickness
- Melting Point
- Maximum Service Temperature, Air
- MgO Content
- Water Leachable Elements on Surface of Fiber, PPM
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|