Thermal Ceramics Kaowool Wet Felt

 

Subcategory: Kaolin

Material Notes:
Thermal Ceramics Kaowool Wet Felt is manufactured by combining Kaowool ceramic fiber with an inorganic bonding agent. It is very pliable with good green strength. Wet Felt may be cut into any size or shape, or it may be formed or molded. It will conform to any surface or contour. When dried or fired, it becomes a lightweight resilient insulator which can be sawed, cut, or sanded. It will not crack or spall or be wet by molten aluminum.

Kaowool Wet Felt is a highly efficient insulator. Its longer fibers give it the high tensile strength and resiliency to withstand vibration and physical abuse. Kaowool Wet Felt has low thermal conductivity, low heat storage, and is extremely resistant to thermal shock.

Features:

  • Highly efficient insulator
  • Good green strength and may be formed or molded
  • Completely inorganic
  • Applications:

  • Line trough and areas contacted with molten aluminum
  • Interior of dryers
  • Curved areas in ovens
  • Insulation for pipe wrap
  • Information provided by Thermal Ceramics

    Available Properties
    • Density
    • Permeability
    • Thickness
    • Modulus of Rupture
    • Melting Point
    • Maximum Service Temperature, Air
    • Shrinkage
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。