Thermal Ceramics TR-19 Block Insulation

 

Material Notes:
TR-19 Block is an asbestos-free insulation products, manufactured from vermiculite granules and high temperature bonding materials. Because of its low conductivity, TR-19 Block is an economical, energy saving insulation. It exhibits minimal shrinkage at its 1900°F (1040°C) temperature limit, and will not readily decompose even when exposed directly to flame or cryolite vapor conditions.

Features:

  • Low thermal conductivity
  • Block construction 36" x 12"
  • Good high temperature strength
  • Variety of thicknesses up to 7”
  • Resistant to cryolite vapors

    Curved Block

  • Designed for curved or circular equipment
  • TR-19 recommended for temperatures up to 1900°F

    Applications:

  • Side and end wall insulating material in carbon baking pits
  • Backup insulation in aluminum pot cells, reheat and pusher furnaces, copper reverberatory furnaces, and oil-fired water tube boilers

    Curved Block

  • Interior and exterior use on bustle pipes, hot air pipes, stacks and other curved or circular equipment
  • Information provided by Thermal Ceramics

    Available Properties
    • Density
    • Loss On Ignition
    • Porosity
    • Modulus of Rupture
    • Compressive Strength
    • Specific Heat Capacity
    • Thermal Conductivity at Elevated Temperature
    • Maximum Service Temperature, Air
    • Shrinkage
    • Sulfur Trioxide Content, %
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。