Thermal Ceramics Kaocrete 32-CM Dense Castables
Subcategory: Kaolin
Material Notes: Kaocrete 32-CM is a 3200°F (1760°C), casting grade, refractory castable with a 70% alumina content. It possesses excellent volume stability and high strength.Features: Recommended use limit up to 3000°F (1649°C) Aggregate chemistry and grain sizing High purity binder systems Installed by cast, gun or plaster Applications: Around water-cooled boiler tubesBoiler ash hoppersKiln carsPiersCar bottomsSeal tanks in FCCU vessels Burner blocksLadle metallurgy lance materialInformation provided by Thermal Ceramics
| Available Properties |
- Density
- Modulus of Rupture
- Compressive Strength
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Shrinkage
- Shelf Life
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|