Thermal Ceramics Kaogun 28 Dense Gunning Castables
Subcategory: Kaolin
Material Notes: Kaogun 28 is a general purpose 2800°F (1538°C) guniting castable with minimal rebound. The combination of an intermediate-purity, calcium-aluminate cement, and a low-porosity calcined kaolin produces excellent performance at an economical price. A typical application would be reheat furnace roof and side wall repair.Applications Hot and cold gunning repairExisting refractory and ash hoppersReheat furnace roof and side wall repair Forging furnace liningsInformation provided by Thermal Ceramics
| Available Properties |
- Density
- Modulus of Rupture
- Compressive Strength
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Shrinkage
- Shelf Life
|
|
|
|