Thermal Ceramics Kaolite 2200 Gunning Insulation Castables
Subcategory: Kaolin
Material Notes: Kaolite 2200 Gun is a lightweight castable designed for temperatures up to 2200°F (1204°C). It has excellent volume stability, good strength, and low thermal conductivity.Information provided by Thermal Ceramics
| Available Properties |
- Density
- Modulus of Rupture
- Compressive Strength
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Shrinkage
- Shelf Life
|
|
|
|