Thermal Ceramics Kaolite 2200-HS Gunning Insulation Castables
Subcategory: Kaolin
Material Notes: Kaolite 2200-HS Gun is a high-strength, lightweight castable designed for easy gunite placement (very low rebound). Kaolite 2200-HS Gun has excellent volume stability up to 2200°F (1204°C) and good abrasion resistance for an insulating castable. It possesses the best thermal onductivity-to-weight ratio in the industry.Information provided by Thermal Ceramics
| Available Properties |
- Density
- Modulus of Rupture
- Compressive Strength
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Shrinkage
- Shelf Life
|
|
|
|