Thermal Ceramics Kaolite 1:2:4 Super Lightweight Insulating Castables
Subcategory: Kaolin
Material Notes: Super lightweight Kaolite castables reduce both the quantity of heat storage and heat transfer through the lining producing significant savings in furnace fuel consumption. The lower densities of these vermiculite based Kaolite castables reduce the amount of supporting furnace steel work required and provide more insulation with a thinner lining. These products can be cast, poured, or gunited. Kaolite 1:2:4 is a general-purpose, lightweight castable for use up to 2000°F (1093°C). It maintains excellent volume stability throughout its temperature use range. This is an excellent advantage for applications where strength and low thermal conductivity are required. Information provided by Thermal Ceramics
| Available Properties |
- Density
- Modulus of Rupture
- Compressive Strength
- Thermal Conductivity
- Maximum Service Temperature, Air
- Shrinkage
- Shelf Life
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|