Thermal Ceramics Kaolite 3300 High Temperature Insulating Castables
Subcategory: Kaolin
Material Notes: Kaolite 3300 is a high strength bubble alumina, lightweight castable with a high-purity binder. It contains less than 0.2% iron oxide and 0.5% silica. Kaolite 3300 is recommended for transfer lines to secondary ammonia reformers, and other applications where resistance to hydrogen atmospheres and silica pickup is critical.Features: Low thermal conductivity Reduction of the quantity of heat storage and heat transfer produce significant savings in fuel consumptionTemperature range up to 3300°F (1816°C)Information provided by Thermal Ceramics
| Available Properties |
- Density
- Modulus of Rupture
- Compressive Strength
- Thermal Conductivity
- Maximum Service Temperature, Air
- Shrinkage
- Shelf Life
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|