Thermal Ceramics Kao-Tab 95 Gun High Alumina Castables
Subcategory: Oxide, Aluminum; Oxide
Material Notes: Kao-Tab 95 Gun is a 95%-alumina castable designed for gunning. It maintains high strength throughout the temperature range of 3400°F (1871°C). Key features are high strength, high-use limit, good slag resistance, and high purity.Features: Designed for supercritical applications Specially enhanced high alumina chemistries that allow Kao-Tab to outperform conventional castables Applications: Cat cracker transfer lines where more abrasion resistance is needed Secondary ammonia reformer linings where low silica is desiredRecovery boiler Upper furnace walls Recovery/cyclone boilers Lower furnace walls and floor Cyclone boilersInformation provided by Thermal Ceramics
| Available Properties |
- Density
- Modulus of Rupture
- Compressive Strength
- Abrasion
- Thermal Conductivity
- Maximum Service Temperature, Air
- Shrinkage
- Shelf Life
- MgO Content
- TiO2 content
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|