Thermal Ceramics Kao-Tab HDHS-98 High Alumina Castables
Subcategory: Oxide, Aluminum; Oxide
Material Notes: Kao-Tab HDHS-98 is a very high purity, 98% alumina castable with high hot strengths. Excellent for hydrogen atmospheres needing high-purity or high temperature applications in the ion and steel, chemical processing, and cement industries.Features: Designed for supercritical applications Specially enhanced high alumina chemistries that allow Kao-Tab to outperform conventional castables Applications: Cat cracker transfer lines where more abrasion resistance is needed Secondary ammonia reformer linings where low silica is desiredRecovery boiler Upper furnace walls Recovery/cyclone boilers Lower furnace walls and floor Cyclone boilersInformation provided by Thermal Ceramics
| Available Properties |
- Density
- Modulus of Rupture
- Compressive Strength
- Abrasion
- Thermal Conductivity
- Maximum Service Temperature, Air
- Shrinkage
- Shelf Life
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|