Thermal Ceramics Kaocrete 249 C Low Cement Castables
Material Notes: Kaocrete 249C is a low cement castable designed for internal or external high frequency vibration placement. It provides excellent volume stability and load bearing characteristics for continuous operation of 2800°F (1538°C). Features: High-strength low cement castables Closely controlled grain sizing Rival the low porosity and low hot load deformation of many dense firebricks Applications: Forge furnace hearths Door jambs Lintels and piers Cartops Rotary kiln nose rings, retainer rings and dams Rotary hearth curbs Walking beam furnace hearth Pusher furnace hearths Skid pipe protection Troughs for molten copperInformation provided by Thermal Ceramics
| Available Properties |
- Density
- Porosity
- Deformation
- Modulus of Rupture
- Compressive Strength
- Abrasion
- Thermal Conductivity
- Maximum Service Temperature, Air
- Shrinkage
- Shelf Life
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|