Thermal Ceramics Kaocrete 250 C Low Cement Castables
Material Notes: Kaocrete 250C is a high-density, high-strength 3200°F (1760°C) low cement castable with excellent thermal shock resistance and good volume stability. Its low iron content and high hotstrengths provide excellent performance in extreme service conditions. General applications would be
precast burner blocks and precast shapes. Features: High-strength low cement castables Closely controlled grain sizing Rival the low porosity and low hot load deformation of many dense firebricks Applications: Forge furnace hearths Door jambs Lintels and piers Cartops Rotary kiln nose rings, retainer rings and dams Rotary hearth curbs Walking beam furnace hearth Pusher furnace hearths Skid pipe protection Troughs for molten copperInformation provided by Thermal Ceramics
| Available Properties |
- Density
- Porosity
- Deformation
- Modulus of Rupture
- Compressive Strength
- Abrasion
- Thermal Conductivity
- Maximum Service Temperature, Air
- Shrinkage
- Shelf Life
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|