Thermal Ceramics R Pyro-Log Fiber

 

Material Notes:
Pyro-Log is an uncompressed monolithic mass of ceramic fiber. Pyro-Log fiber is available in 6" and 8" (152 mm to 203 mm) thicknesses with densities up to 15 pcf (240 kg/m3). Manufactured in three temperature grades, R, ZR and C, the Pyro-Log fiber can be used in a wide range of applications. Pyro-Log fiber is the basic building block for all Pyro-Bloc applications.

All Pyro-Log fiber is produced with a special lubricant that allows the fibers to be intensely needled to attain densities up to 15 pcf (240 kg/m 3). This lubricant also adds pliability which allows true ultidirectional compression during installation. At moderate temperatures this lubricant burns out and the fiber becomes rigid enough to stand on. This feature, unique to Pyro-Log fiber, assists during installation and provides the durability and toughness necessary for long life.

Features:

  • Monolithic log of 6” to 8” (152 mm to 203 mm) thick refractory ceramic fiber
  • Available densities up to 15 pcf (240 kg/m3)
  • Fully needled - no adhesives
  • Applications:

  • Low mass kiln cars
  • Fired heater floors
  • Back up insulation for insulating firebrick and castable lining
  • Fill gaps or small spaces where standard shapes are not practical
  • Information provided by Thermal Ceramics

    Available Properties
    • Density
    • Thermal Conductivity
    • Melting Point
    • Maximum Service Temperature, Air
    • Other Element Content
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。