Thermal Ceramics HS Pyro-Bloc Module
Material Notes:
Features: Next evolution in ceramic fiber Designed for enhanced mechanical abuse resistance Proprietary hardening agent Compressible in its green state Enhanced hardness upon minimal temperatures Available in “Y”, “M” and “T-bar” attachments systems Applications: Stack linings Flare linings Ductwork linings Kiln car block Kiln car seals Burner block Peep sights Corbell block Convection section Fluidized bed unitsInformation provided by Thermal Ceramics
| Available Properties |
- Density
- Thickness
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |