Thermal Ceramics Board FireMaster
Material Notes: FireMaster Board is classified by Underwriters Laboratories under “Mineral and Fiber Boards (BQXR)” in the UL Building Materials Directory, No. R9073. FireMaster Board is manufactured to ensure continued compliance with certification standards. Features: UL-classified, noncombustible material Rigid, lightweight Good thermal and sound attenuation properties Good tensile and compressive strengths Resists chemical attack Unaffected by oil or waterApplications: Decking Fire doors Wall and ceiling applications Vaults Firestop damming material Above ground storage tanksInformation provided by Thermal Ceramics
| Available Properties |
- Density
- Modulus of Rupture
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Flammability Test
- Comprehensive Strength
- Thermal Resistance, R value
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|