Thermal Ceramics Door Seal+ FireMaster
Material Notes: FireMaster Door Seal+ is an intumescent material produced from a unique blend of high-purity, high temperature fibers, special additives, and binders in a special process. At maximum expansion which occurs at approximately 1200°F (649°C), the FireMaster Door Seal+ expands up to 800% of its thickness. This results in the FireMaster Door Seal+ being an excellent candidate for high-temperature gaskets and seals. Like all the other high-quality FireMaster products, FireMaster Door Seal+ is noted for its excellent flexibility, outstanding handling characteristics, and high-insulating value. Features: 2000°F (1093°C) capability Lightweight, flexible, simple to cut and install Expands 8 times its thickness UL CLBV R17035 Withstands ASTM E 119, IMO A.754 and , UL-1709 Low biopersistent composition Applications: Fire doors Expansion joints Marine bulkhead and decks Military bulkhead and decks Offshore Platform bulkhead and decks Gaskets and seals OEM manufactured systemsInformation provided by Thermal Ceramics
| Available Properties |
- Density
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|