Thermal Ceramics SR-99 LS Firebrick
Material Notes: The SR-90, SR-99, and SR-99 firebricks are premium high alumina firebricks that are capable of handling very difficult applications. These premium bricks are very dense and have excellent load bearing strength at temperatures above 3000°F (1649°C) and they provide excellent thermal shock resistance. The extremely low silica content of both products make them ideal for hydrogen atmospheres.Features: 90 and 99% alumina firebrick Excellent low SiO2 contents for use in Hydrogen atmospheres Excellent high temperature stability Extremely high service temperatureApplications: Sulphur recovery unitsIncinerators Secondary ammonia reformersInformation provided by Thermal Ceramics
| Available Properties |
- Density
- Deformation
- Modulus of Rupture
- Compressive Strength
- Thermal Conductivity
- Shrinkage
- Fe2O3
- MgO Content
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|