Thermal Ceramics JM-26 High Temperature Insulating Firebrick

 

Material Notes:
Thermal Ceramics high temperature insulating firebrick are produced with unique processes. The bond developed is a ceramic bond that is formed by high temperature firing. This produces bricks that are very stable and strong at temperatures higher than 2600°F (1427°C).

Features:

  • High temperature insulating firebrick with use limits up to 3250°F (1788°C)
  • Excellent strength and thermal stability
  • Low heat storage
  • High purity
  • Excellent thermal conductivity
  • Applications:

  • Atmosphere furnace
  • Forge furnaces
  • Ethylene furnace sidewalls
  • Ceramic kilns
  • High temperature back-up insulation
  • Carbon baking furnaces
  • High temperature kiln linings
  • Removable furnace doors
  • Information provided by Thermal Ceramics

    Available Properties
    • Density
    • Deformation
    • Modulus of Rupture
    • Compressive Strength
    • Thermal Conductivity
    • Maximum Service Temperature, Air
    • Shrinkage
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。