Thermal Ceramics K-20 Low Temperature Insulating Firebrick

 

Material Notes:
Thermal Ceramics was first to introduce insulating firebrick (IFB) to the industry in the 1930’s. The IFB are manufactured with a unique slurry casting process which creates a network of microporosity which produces low thermal conductivity and good thermal shock characteristics. This process produces brick that are some of the most efficient insulators available in the market. The anorthite mineralogy (CaO, Al2O3, 2 SiO2) of these low temperature IFB gives them excellent strength at operating temperatures and resistance to corrosive alkali environments.

Features:

  • Extremely low “K” factors
  • Low densities
  • Low heat storage
  • Excellent strength at room and high temperatures
  • Excellent resistance to alkali attack
  • Excellent service in applications involving special atmospheres
  • Applications:

  • Backup insulation for carbon baking furnaces
  • Backup insulation in aluminum electrolytic cells
  • Electrical kilns for industrial and hobby use
  • Backup insulation for blast furnace stove linings
  • Linings for carbonizing furnaces
  • Forge furnace linings
  • Heat transfer linings
  • Information provided by Thermal Ceramics

    Available Properties
    • Density
    • Deformation
    • Modulus of Rupture
    • Compressive Strength
    • Thermal Conductivity
    • Melting Point
    • Maximum Service Temperature, Air
    • Shrinkage
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。