Thermal Ceramics 100 Cerox Shapes
Material Notes: Cerox fired refractory shapes are thixotropically cast using a dispersion agent, which allows the Cerox mix to flow when vibrated without requiring a high water content. These manufacturing techniques, combined with precisely controlled firing and 100% product inspection, produce high-quality components suited to the most arduous of high-temperature environments. Features: Variety of available compositions using high-alumina, alumina-silica, zirconia, and silicon carbide Excellent chemical attack resistance Excellent thermal shock resistance Low gas permeability Hundreds of standard molds in stock Tight tolerance capabilityApplications: Process Industries (chemical & mineral processing) combustion chambers burner blocks pipes gas reactor components wear plates crucibles nozzles resistance heater hangers, holders, etc.Metals (steel & special alloy) runners pipes induction blocks crucibles tundish boxes distribution plates combustion components skid rails rabble blocks and teeth nozzles Technical Ceramics (ceramic industry & OEM furnace builders) saggers setters pusher tiles tubes plates crucibles muffles skid rails piersInformation provided by Thermal Ceramics
| Available Properties |
- Bulk Density
- Porosity
- Permeability
- Modulus of Rupture
- CTE, linear 68°F
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|